It depends the some cast manifolds are prone to cracking, and are rough as a badgers bum inside which reduces the flow rate and generates excess heat through friction, the stainless one tend to flow better, and get up to temp quicker reducing the cracking possibilities.
swings and round abouts, the cast ones can be smothed inside witha dremell or simillar tool.